Clinker production: the feed stock first enters the raw material to make a fine powder where 85% of the material is less than 88 μm. Then, the feed is transferred to the homogenizing silos. Afterwards, the meal is thrown into the precalciner tower to start the chemical change to cement. Towers mixes homogenous feed with exhaust kiln gas to recover energy at almost 1000°C .