The laminate is peeled apart at an angle of 180° with a jaw separation speed of 300 mm per minute. The average force is recorded from the centre section of the test strip from at least 5 readings at 10 mm intervals. Fix each strip to the test plate with doublesided tape. The facing material can be peeled from the release substrate, or vice versa.