J. Lehto, in Encyclopedia of Separation Science, 2000 Ion Exchange in the Processing of Uranium Ores. Uranium ores are first ground into submillimetre particles and uranium is leached out with sulfuric acid. If the ore contains a large quantity of acidconsuming CaCO 3, leaching is carried out with sodium or ammonium carbonate sulfuric acid and carbonate .